Заглавие Oxidation of titanium carbide-graphite hetero-modulus ceramics with low carbon content. I. Phenomenological modeling of the ridge effect
 
Автор Shabalin, I. L.
Roach, D. L.
Shabalin, L. I.
 
Тематика CARBON
CHEMICAL PROPERTIES
COMPOSITES
HETERO-MODULUS CERAMICS
TIC
ACTIVATION ENERGY
BUILDING MATERIALS
CARBON
CERAMIC MATERIALS
ELASTIC MODULI
ELASTICITY
GRAPHITE
MATERIALS PROPERTIES
METALLIC MATRIX COMPOSITES
OXYGEN
TITANIUM
TITANIUM CARBIDE
TITANIUM COMPOUNDS
CHEMICAL PROPERTIES
COMPOSITES
HETERO-MODULUS CERAMICS
TIC
YOUNG'S MODULUS
OXIDATION
 
Описание Hetero-modulus ceramic composite materials (HMC) present an opportunity to combine a ceramic matrix having high Young's modulus with inclusions of a material having a considerably lower value of Young's modulus, resulting in a material with significantly improved properties. The isobaric-isothermal oxidation of 93 vol.% TiC-7 vol.% C (graphite) hot-pressed HMC was studied at temperatures of 400-1000 °C and pressures of 0.13-65 kPa in oxygen flow using a microbalance. The TGA data and carbon content analysis of oxidised samples were applied in the kinetics phenomenological modeling for both carbon burn-off and oxygen consumption processes. The activation energies Q and orders of reaction m were determined for all oxidation parameters and stages of the process, described using a linear-paralinear model. The oxidation behaviour of the material is characterised by the presence of a so-called "ridge effect". The ridge temperature and ridge oxygen pressure serve as boundaries between regions defined by higher or lower values of oxidation parameters and mark a change in the prevailing oxidation mechanism, as while traversing the ridge parameter the values of Q and m change their sign. © 2008 Elsevier Ltd. All rights reserved.
 
Дата 2019-07-17T10:00:19Z
2019-07-17T10:00:19Z
2008
 
Тип Article
Journal article (info:eu-repo/semantics/article)
Published version (info:eu-repo/semantics/publishedVersion)
 
Идентификатор 0955-2219
https://www.scopus.com/record/display.uri?origin=resultslist&eid=2-s2.0-51749123543
https://elar.rsvpu.ru/handle/123456789/28147
10.1016/j.jeurceramsoc.2008.04.035
51749123543
2-s2.0-51749123543
Institute for Materials Research, The University of Salford, Greater Manchester M5 4WT, United Kingdom
Russian State Professional and Pedagogical University, Yekaterinburg, 620012, Russian Federation
Scopus
Shabalin, I.L., Institute for Materials Research, The University of Salford, Greater Manchester M5 4WT, United Kingdom
Roach, D.L., Institute for Materials Research, The University of Salford, Greater Manchester M5 4WT, United Kingdom
Shabalin, L.I., Russian State Professional and Pedagogical University, Yekaterinburg, 620012, Russian Federation
WOS:000260276300021
000260276300021
 
Язык en
 
Права Restricted accedd (info:eu-repo/semantics/restrictedAccess)
 
Формат text/html
 
Охват RSVPU
SCOPUS
 
Издатель Elsevier BV
 
Источник Journal of the European Ceramic Society
 
##plugins.schemas.dc.fields.audience.name## Other
Parents and Families
Researchers
School Support Staff
Students
Teachers